Moisture map of North America showing average moisture content ranges for interior wood in each US state, Canadian province, and Mexican state

Obrázek z NWFA. Reprodukováno s laskavým svolením.

This EMC chart of North America shows the average moisture content (MC) ranges for wood used indoors in each region. Use it as a starting point for the MC you can expect for interior wood in your area.

As the note on the map explains, these numbers are examples of how average moisture content for interior wood products varies from one region to another and from one season to another within a region. Actual moisture content conditions in any location may differ significantly from these numbers.

To estimate the equilibrium moisture content (EMC) for a specific temperature and relative humidity, use our Kalkulačka EMC. Then check the wood itself with an accurate moisture meter.

Zjistěte vše o Co je EMC a vzorec v našem průvodci.